Introduction:
Fiberglass geogrid is knitted by glass fiber filaments and coated with bitumen to provide a good bond with the asphalt layers, can strengthen the asphalt layer, extend the service life ot pavement layers and decrease the occurrence rate of reflective cracking under cyclic traffic load.
Data Sheet
Property | Test method | TGSB 30-30 | TGSB 40-40 | TGSB 50-50 | TGSB 60-60 | TGSB 70-70 | TGSB 80-80 | TGSB 90-90 | TGSB 100-100 | TGSB 120-120 | TGSB 130-130 | ||
Ultimate tensile strength | KN/m | MD | EN ISO 10139 | 30 | 40 | 50 | 60 | 70 | 80 | 90 | 100 | 120 | 130 |
CD | 30 | 40 | 50 | 60 | 70 | 80 | 90 | 100 | 120 | 130 | |||
Elongation at maximum load | % | MD | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | |
CD | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | |||
Approximate mesh size | mm | 12-50 | |||||||||||
Roll width | m | 1-6 | |||||||||||
Roll length | m | 50-200 |
Application:
1. The old asphalt concrete pavement is reinforced to strengthen the asphalt surface layer to prevent diseases.
2. The cement concrete pavement is converted into a composite pavement to suppress reflection cracks caused by plate shrinkage.
3. Road extension and improvement project to prevent cracks caused by the junction of new and old and uneven settlement.
4. Reinforcement treatment of soft soil foundation is conducive to the consolidation of soft soil water separation, effectively inhibits settlement, uniform stress distribution, and enhances the overall strength of the roadbed.
5. The semi-rigid base of the newly built road produces shrinkage cracks, and the reinforcement is reinforced to prevent the pavement cracks caused by the reflection of the base cracks.
FAQ
1, What is the difference between uniaxial and biaxial geogrid?
Biaxial geogrids are those that exhibit the same strength in both the machine directions MD and cross-machine directions CMD while uniaxial geogrids exhibit the primary strength in the machine direction with minimal strength, enough to maintain the aperture structure, in the cross-machine direction.
2, How many types of geogrids are there?
There are three different types of geogrids: Uniaxial, Biaxial, and Triaxial . Each one is designed and manufactured for specific construction applications with various tensile strengths.
3, Are you trading company or manufacturer?
We are factory.
4,Is the quality of your products stable?
The company has a complete QC system, and each batch of products will be sampled and the samples will be kept for 5 years.
5,Can you do OEM?
Yes, of course. We can produce the products as your request.
Introduction:
Fiberglass geogrid is knitted by glass fiber filaments and coated with bitumen to provide a good bond with the asphalt layers, can strengthen the asphalt layer, extend the service life ot pavement layers and decrease the occurrence rate of reflective cracking under cyclic traffic load.
Data Sheet
Property | Test method | TGSB 30-30 | TGSB 40-40 | TGSB 50-50 | TGSB 60-60 | TGSB 70-70 | TGSB 80-80 | TGSB 90-90 | TGSB 100-100 | TGSB 120-120 | TGSB 130-130 | ||
Ultimate tensile strength | KN/m | MD | EN ISO 10139 | 30 | 40 | 50 | 60 | 70 | 80 | 90 | 100 | 120 | 130 |
CD | 30 | 40 | 50 | 60 | 70 | 80 | 90 | 100 | 120 | 130 | |||
Elongation at maximum load | % | MD | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | |
CD | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | |||
Approximate mesh size | mm | 12-50 | |||||||||||
Roll width | m | 1-6 | |||||||||||
Roll length | m | 50-200 |
Application:
1. The old asphalt concrete pavement is reinforced to strengthen the asphalt surface layer to prevent diseases.
2. The cement concrete pavement is converted into a composite pavement to suppress reflection cracks caused by plate shrinkage.
3. Road extension and improvement project to prevent cracks caused by the junction of new and old and uneven settlement.
4. Reinforcement treatment of soft soil foundation is conducive to the consolidation of soft soil water separation, effectively inhibits settlement, uniform stress distribution, and enhances the overall strength of the roadbed.
5. The semi-rigid base of the newly built road produces shrinkage cracks, and the reinforcement is reinforced to prevent the pavement cracks caused by the reflection of the base cracks.
FAQ
1, What is the difference between uniaxial and biaxial geogrid?
Biaxial geogrids are those that exhibit the same strength in both the machine directions MD and cross-machine directions CMD while uniaxial geogrids exhibit the primary strength in the machine direction with minimal strength, enough to maintain the aperture structure, in the cross-machine direction.
2, How many types of geogrids are there?
There are three different types of geogrids: Uniaxial, Biaxial, and Triaxial . Each one is designed and manufactured for specific construction applications with various tensile strengths.
3, Are you trading company or manufacturer?
We are factory.
4,Is the quality of your products stable?
The company has a complete QC system, and each batch of products will be sampled and the samples will be kept for 5 years.
5,Can you do OEM?
Yes, of course. We can produce the products as your request.